Mar 13, 2023 Ostavite poruku

Cause and analysis of surface corrosion of aluminum extruded profiles

In the process of surface treatment of 6063 aluminum alloy profiles, it is sometimes found that there are different degrees of irregular arrangement of spot-like dark gray corrosion points on the surface of aluminum profiles. The shape of the corrosion points is completely different from that caused by zinc elements, and it is intermittent in the production process of aluminum profiles. Some people think the reason is that the operator did not perform the correct surface treatment process; There are some harmful impurity ions in the tank. Bad material, too much inclusion. In this regard, we analyze as follows.

1. Cause analysis of corrosion points

 

Based on many years of production experience and investigation of various process parameters in the production of aluminum alloy profiles, as well as follow-up investigation of the operator's execution of the process, we believe that the main reasons for this type of dark gray corrosion point are as follows:

 

(1) Sometimes because of some reasons in the casting process of magnesium, silicon addition ratio is not appropriate, so that ω(Mg)/ω(Si) in the range of 1.0 ~ 1.3, much smaller than the best ratio of 1.73 (generally controlled in the range of 1.3 ~ 1.5). So although magnesium, silicon content in rules (omega (Mg) = 0.45% ~ 0.9%, omega (Si) = 0.2% ~ 0.6%). However, there is some excess silicon, which can form ternary compounds in aluminum alloy at the same time except for a small amount of silicon in the free state. When ω(Si)<ω(fe), more="" α(al12fe3si)="" phase="" is="" formed,="" which="" is="" a="" brittle="" compound,="" and="" when="" ω(si)=""> ω(Fe), more β(Al9Fe2Si12) phase is formed, which is a more brittle needle-like compound, which has more harmful effects than the α phase, and tends to make the alloy easily fracture along it. These insoluble impurity phases or free impurity phases formed in the alloy tend to gather at the grain boundary, and weaken the strength and toughness of the grain boundary [1-3], becoming the weak link with the worst corrosion resistance, and corrosion occurs from there first.

 

(2) in the process of smelting, although the proportion of adding magnesium and silicon in within the prescribed scope of the standard, but sometimes because of the uneven mixing and inadequate, causing uneven distribution of silicon in the melt, local enrichment region and poor area. Because the solubility of silicon in aluminum is very small, the eutectic temperature is 1.65% at 577℃ and only 0.05% at room temperature, the phenomenon of uneven composition occurs after casting rods, which is directly reflected in the industrial aluminum products. When there is a small amount of free silicon in the aluminum matrix, the corrosion resistance of the alloy is reduced, and the grain of the alloy is coarsened [4].

 

(3) The control of various process parameters during extrusion, such as too high preheating temperature of bar billet, improper control of metal extrusion flow rate, air cooling strength during extrusion, aging temperature and holding time, are easy to produce silicon segregation and ionization, so that magnesium and silicon do not completely form Mg2Si phase, but some free silicon exists.